Best Low temperature Brazing Alloys
20 Sticks BLUEFIRE JAgP-5 1/2 lb 5% Silver Phos Copper Brazing Alloys Welding Rods Industry BCuP-3 0.050\x1/8\x14\ equivalent to HARRIS STAY SILV 5 Professional Grade Gas Soldering Torch Accessory
- 5% Silver Bearing: USA AWS A58 Class: BCuP-3 brazing alloys rods. Contents: Silver (Ag) 4.8-5.2%.
- Copper (Cu): Rest. For the best results, recommend to be use with Bluefire JFB-102S brazing flux..
- Valued Pack: Each tube contains 20 sticks of 14" long brazing rods, total 0.5 (1/2) pound in weight. GREAT SAVING!.
- Best Performances: Solidus Temperature: 1189°F / 643°C, Liquidus Temperature: 1419°F / 771°C. Recommended Joint Clearance: 0.003"/0.006.
Check StockK-T Industries 2-2750 Brazing Flux, 0.5 lb
- Price For: Each Tensile Strength (PSI): - Type: - Contents: 56% Silver, 22% Copper, 17% Zinc, 5% Tin Container: - Application: For Ferrous and Non Ferrous Alloys Good for Stainless Steel Includes: 1 oz Brazing Wire and 1.75 oz White Flux Item: Brazing Kit Material: Safety-Silv-56 Dia. (In.): 1/16 Length (In.): - Brazing Range (F): 1145 to 1205 Standards: AWS A5.8, Bag-7, NSF 51.
- Country of Origin (subject to change): United States.
Check StockRBCuZn-C - LFB Bare Bronze Brazing Rod - 36 x 1/8 1 Lb
- LFB (bare low fuming bronze) is a general purpose oxyacetylene/brazing rod used for joining various ferrous and non-ferrous metals such as carbon steel, copper alloys, cast iron, malleable iron, stainless steel and some nickel alloys. Mechanical and physical characteristics include ductility, machineability, high strength, free flowing with good tinning action and a low melting point (1630°F).
- A “must have” filler metal for every machine shop, LFB is excellent for building up wearing surfaces or large areas where successive layers must be added.
- galvanized parts can be brazed without damaging the zinc coating. Precise balance of copper and zinc along with alloying elements of tin, iron, manganese and silicon produces weld deposits that can be easily machined but work harden once put into service.
- READ THIS: Main image is for reference only. Please check Picture #2 for an approximate quantity of rods per pound***.
- Available in different sizes: 0.045", 1/6", 3/32", 1/8", 5/32", 3/16" and 1/4".
- Available in different package weights: 1 Lb, 2 Lb, 5 Lb and 10 Lb.
Check StockAufhauser SilverAlloy 45% Ag BAg-5 18 Flux Coated Silver Solder Brazing Rods 3 Sticks
- Fluxed coated Cadmium-free 45% Silver brazing rods. 1/16" Core (3 Sticks).
- For general purpose brazing of ferrous and non-ferrous alloys excluding aluminum..
- For joining and repairing of Copper, Brass, Steel, Stainless Steel and Cast Iron..
Check StockAufhauser SilverAlloy 56% Ag BAg-7 1/16 x 18 Flux Coated Silver Solder Brazing Rods 3 Sticks
- Fluxed coated 56% Silver brazing rods, 1/16" Core. (3 Sticks).
- For general purpose brazing of ferrous and non-ferrous alloys excluding aluminum..
- For joining and repairing of Copper, Brass, Steel, Stainless Steel and Cast Iron..
- Meets AWS A5.8 BAg-7. AMS 4763, QQB-654A Class BAg-7.
Check StockBernzomatic PC3 Copper-Phosphorous Brazing/Welding Rods, 3-Piece
- Copper-phosphorous brazing/welding rods ideal for use in refrigeration, electrical and plumbing jobs.
- Working temp: 1,310-1,475-Degree farenheit.
- Joins copper to copper without flux, or copper to copper alloys (brass, and bronze).
Check StockCynKen 1x200x200mm Titanium Plate Sheet TA2/GR2 Sheet
- High strength - density titanium alloy generally about 4.5g / cm3..
- High heat intensity - temperature of several hundred degrees higher than aluminum..
- Good corrosion resistance - Titanium work in a humid atmosphere and seawater, the corrosion resistance is far superior to stainless steel.
- for pitting, etching, stress resistance particularly strong.
- and other organic materials have excellent corrosion resistance..
- Good low temperature performance titanium alloys at low temperatures and extremely low temperatures, can still maintain its mechanical properties..
Check StockCynKen 1x100x100mm Titanium Plate Sheet TA2/GR2 Sheet
- High strength - density titanium alloy generally about 4.5g / cm3..
- High heat intensity - temperature of several hundred degrees higher than aluminum..
- Good corrosion resistance - Titanium work in a humid atmosphere and seawater, the corrosion resistance is far superior to stainless steel.
- for pitting, etching, stress resistance particularly strong.
- and other organic materials have excellent corrosion resistance..
- Good low temperature performance titanium alloys at low temperatures and extremely low temperatures, can still maintain its mechanical properties..
Check StockCynKen 2x100x100mm Titanium Plate Sheet TA2/GR2 Sheet
- High strength - density titanium alloy generally about 4.5g / cm3..
- High heat intensity - temperature of several hundred degrees higher than aluminum..
- Good corrosion resistance - Titanium work in a humid atmosphere and seawater, the corrosion resistance is far superior to stainless steel.
- for pitting, etching, stress resistance particularly strong.
- and other organic materials have excellent corrosion resistance..
- Good low temperature performance titanium alloys at low temperatures and extremely low temperatures, can still maintain its mechanical properties..
Check StockCynKen 2x200x200mm Titanium Plate Sheet TA2/GR2 Sheet
- High strength - density titanium alloy generally about 4.5g / cm3..
- High heat intensity - temperature of several hundred degrees higher than aluminum..
- Good corrosion resistance - Titanium work in a humid atmosphere and seawater, the corrosion resistance is far superior to stainless steel.
- for pitting, etching, stress resistance particularly strong.
- and other organic materials have excellent corrosion resistance..
- Good low temperature performance titanium alloys at low temperatures and extremely low temperatures, can still maintain its mechanical properties..
Check StockCynKen 0.5x200x200mm Titanium Plate Sheet TA2/GR2 Sheet
- High strength - density titanium alloy generally about 4.5g / cm3..
- High heat intensity - temperature of several hundred degrees higher than aluminum..
- Good corrosion resistance - Titanium work in a humid atmosphere and seawater, the corrosion resistance is far superior to stainless steel.
- for pitting, etching, stress resistance particularly strong.
- and other organic materials have excellent corrosion resistance..
- Good low temperature performance titanium alloys at low temperatures and extremely low temperatures, can still maintain its mechanical properties..
Check StockFox Alloy 20pcs Copper Brazing Rods BCuP-2 (5/64\) 2mm Phosphor Round Self Fluxing Copper Welding Rods Sticks TIG Arc Pipes for Air Conditioner Refrigerators
- Material: The package includes 20PCS 2.0mm cooper brazing rods BCuP-2 brass welding rod.
- Standard: The copper welding rods kit conforms to AWS A5.8.
- Advantage: The low temperature phosphor copper welding rod is easy to install and remove. Good fluidity during welding, can flow into small space. Low metling point 640-770℃, good fluidity during welding, molten metal can flow to small gaps.
- Application:The stick TIG welding rods is used for brazing of copper & copper alloy in motors, air-conditioners, meters, and refrigeration industry.
- Service: Fox Alloy Time-proven formulation.
- A team of experienced welding engineers ready to answer all your welding questions..
Check StockJ.W. Harris Company 40022 Stay-Silv White Brazing Flux
- It is a powder flux formulated for brazing gold and silver..
- Jar of welding powder brazing flux powder welding cast consumables jewelry weld repair supply.
- There are 250 grams in this jar, which will definitely meet your needs..
- The powder melts at 700 degree centigrade..
- Brazing powder improves the weldability of metal in the process of high temperature welding..
Check Stock